A useful filled-PTFE coupon screen compares identified compounds under the same documented contact and operating conditions, then reports wear, friction and uncertainty separately. Its output is a shortlist for further engineering work, not a service-life prediction or a universal ranking of fillers. Before requesting samples, agree what the screen should distinguish and what evidence will support that decision.
This guide provides an original planning worksheet, not Pengrowth experimental results or a prescribed laboratory procedure. It concerns material coupons before component qualification. Actual shaft-and-bushing assembly testing requires a separate programme. For available component forms, see filled PTFE machined parts.
Define a comparison that answers one material question
Specify the decision in practical terms: for example, whether alternative compounds deserve further investigation under one nominated dry-sliding condition. Identify a reference material representing the current requirement. Keep its formulation and preparation traceable; “standard PTFE” is not an adequate reference identity.
Give each candidate a code linked to the supplier designation, lot, composition information available for release, stock form and machining direction. Similar filler names do not establish identical compounds. Record specimen geometry, contact-face preparation and conditioning. If preparation differs between candidates, identify that difference before treating the results as a material-only comparison.
Decide how repeat runs, order effects and failed specimens will be handled before testing. The laboratory should justify the replication plan against the expected variability and decision sensitivity. No fixed sample count is suitable for every screening request. Retain individual results rather than submitting only a single favourable average.
Select the contact geometry and document the method
ASTM G99-23 addresses pin- or ball-on-disk wear and friction testing. ASTM G133-22 concerns reciprocating ball-on-flat sliding. These are different contact/motion arrangements, not interchangeable labels for a test machine. Agree the applicable method and edition with the laboratory.
The public scope pages are not complete operating procedures. Obtain the actual method where applicable and record any departure. Naming a standard does not demonstrate compliance. A test using selected principles with changed parameters must describe those choices accurately; do not label an improvised experiment “ASTM certified.”
Specify which member of the pair is PTFE, its contact shape and dimensions, the track or stroke, the motion direction and how sliding distance is calculated. A rotating contact and a reversing contact do not share the same velocity history. Avoid comparing their results as if only the compound had changed.
Control the counterface, not just its material name
A counterface description should identify material, relevant hardness or coating, surface-finish measurement, preparation and cleaning. State the measurement direction and parameter used for roughness; two surfaces described merely as “polished steel” are not a controlled comparison. Include photographs or surface records where they help identify the tested condition.
Define whether each run receives a new track or a reused surface. If reuse is allowed, document how the previous contact history is handled. Inspect the surface before and after testing. Any deposits, track damage or cleaning changes belong in the result record, not only in a technician’s notes.
Keep this coupon specification separate from an installed shaft specification. Coupon screening may help select candidate formulations, but it does not approve housing fit, shaft alignment, retention or assembly clearance.
| Control group | Record before testing | If it changes |
|---|---|---|
| Contact pair | Coupon geometry; counterface identity, finish and history | Identify a separate comparison group |
| Mechanical duty | Normal force, motion, speed definition and sliding distance | Do not pool unlike exposures |
| Environment | Measured temperature, humidity where relevant, lubricant and supply condition | Document the actual condition and deviation |
| Measurement | Wear method, friction processing and instrument resolution | Explain whether results remain comparable |
Separate run-in observations from the reporting interval
Preserve the friction trace from the beginning of the run. Define any run-in interval and the rule for reporting a later interval before reviewing candidate results. Do not remove an inconvenient start-up region retrospectively or declare steady behaviour simply because a trace looks flatter.
If the purpose requires a stability criterion, state the measured quantity, observation interval and acceptance rule in the protocol. Report when a specimen never satisfies that rule. Use the same decision logic for the reference and every candidate, and disclose early stops and their reasons.
Photograph the contact and any transferred material at agreed stages where the method permits. Stopping, handling or cleaning can alter a test sequence, so describe these interventions. A visible deposit alone does not prove either favourable wear performance or a particular transfer-film mechanism.
Report wear and friction as different outcomes
Wear quantity and measurement limits
State whether wear is determined by a volume measurement, a mass-change calculation or another justified method. Include the measurement boundary and resolution. If volume is calculated from mass loss, identify the density used for that exact compound; do not use one assumed density for every filled grade. Explain conditioning and cleaning so that retained material or contamination is not silently interpreted as wear.
When reporting a normalized value such as k = V / (F × s), define wear volume V, normal force F and sliding distance s, and give units such as mm³/(N·m). This is an explicit reporting convention, not a universal material constant. State the exposure interval represented. A result below measurement capability should be reported with that limitation, not converted into “zero wear.”
Friction and repeatability
Report how the friction signal was processed, the interval summarized and variability across repeat runs. Separate transient peaks from the selected summary statistic. For reversing motion, explain sign handling and the treatment of reversals. A lower friction summary does not by itself establish lower wear or acceptable counterface damage.
Keep specimen-level results available, including the reference. If differences are small relative to measurement uncertainty or repeat variability, report that the screen does not clearly distinguish those candidates. Avoid manufacturing a rank order from insignificant numerical differences.
Use a blank coupon-screening record
Complete the protocol fields before testing and the results afterward. The following is an original planning tool; it contains no measured data or company acceptance thresholds.
| Field | Agreed protocol | Run record / evidence |
|---|---|---|
| Candidate/reference code, lot and preparation | ________ | ________ |
| Method/edition, geometry and deviations | ________ | ________ |
| Counterface finish, cleaning and track history | ________ | ________ |
| Force, speed/motion, distance and environment | ________ | ________ |
| Run-in rule, reporting interval and stop criteria | ________ | ________ |
| Wear method, units, density if used, resolution | ________ | ________ |
| Friction trace, individual repeats and surface observations | ________ | ________ |
| Uncertainty, exclusions and screening decision | ________ | ________ |
Turn the result into a bounded sourcing decision
The correct conclusion identifies the candidate, reference and conditions under which a difference was observed. ASTM G99 cautions against transferring test wear rates to different service conditions. Retain that boundary when sharing a report with purchasing: coupon evidence can support further evaluation, not a promised replacement interval.
For formulation background, read the PTFE filler comparison. For a supply review, send the candidate designation, coupon or finished-part drawing, quantity, counterface description and proposed screening conditions through the filled PTFE component page. Confirm sample availability and what material documentation can accompany the request. Do not assume an in-house test service or a validated wear value without specific evidence.
Discuss a Filled PTFE Component Requirement
Send the component drawing, load, speed, temperature, counterface, process media, wear concern and quantity for a material and manufacturing review.