Dimensional inspection of extruded PTFE tubing

PTFE Tubing Troubleshooting Guide: Leaks, Kinks, Creep and Surface Damage

Published Updated Technical author

When a PTFE tube leaks or loses flow, the material is not always the root cause. Cutting, routing, fitting selection, temperature, pressure, clamps and contamination can all create similar symptoms. A structured inspection helps separate a dimensional issue from an installation or service problem.

First steps: stop the system safely, record the location and operating conditions, photograph the installed route, preserve the failed tube and fitting, and compare the actual tube dimensions with the drawing.

Common Symptoms and Checks

SymptomPossible causeCheck
Leak at fittingAngled cut, wrong OD, damaged ferrule, side loadCut face, insertion depth, OD and routing
Reduced flowKink, oval bend, deposit or incorrect IDBore through full route
Tube movementThermal expansion, pressure pulse or weak supportTemperature, clamps and cycle
Surface wearRubbing on a sharp edge or vibrationContact points and support spacing
DiscolorationExternal contamination, heat exposure or process residueCleaning history and affected surface

Leaks Near a Fitting

Before loosening a connection or removing tubing, follow the site-authorized isolation, depressurization, cooling and decontamination procedures appropriate to the service. Record the installed position when safe; preserving evidence must not delay an authorized safety response. Check for a square cut, scratches, ferrule marks, insufficient insertion and a bend beginning too close to the connection. Confirm that the fitting matches the actual ID and OD. The PTFE fittings guide provides a connection checklist.

Kinks and Flattened Bends

Compare the installed radius with the free tube. Tight routing, thin wall, heat and twisting can reduce the bore. Follow the authorized response for damaged tubing without delaying necessary replacement or isolation. Investigate and correct routing before returning a replacement to service; otherwise the same damage may recur. See the bend radius guide.

Creep, Sagging and Clamp Marks

PTFE can deform under sustained load. A hot tube, long unsupported span or over-tight clamp may change shape gradually. Use supports that guide without crushing, leave room for thermal movement and inspect the line after realistic operating time.

Abrasion and External Damage

Look for polished areas, grooves or local thinning where the tube contacts metal, cable ties, moving parts or other hoses. Add suitable protection and change the support layout. Do not hide damage under a tighter clamp.

Dimensions and Lot Comparison

Measure ID, OD, wall and cut length using a method appropriate to soft tubing. Compare an unused sample from the same lot, the failed section and the drawing. Use the inspection and traceability records actually agreed and supplied for the order; confirm any missing material, dimensional or lot evidence rather than assuming a check was performed.

Send for failure review:

  • Photos before disassembly
  • Tube and fitting samples
  • Drawing and purchase specification
  • Operating temperature, pressure or vacuum
  • Chemical and cleaning medium
  • Time in service and cycle frequency
  • Failure location and quantity affected

Evidence to Collect Before Replacing the Tube

Troubleshooting is faster when the failed condition is documented before the line is removed. Photograph the entire route and close-ups of fittings, clamps, bends and damaged surfaces. Mark flow direction, failure location and the distance from the nearest connection. Retain the tube, packaging label and production batch information where available.

EvidenceWhat it helps distinguish
Damage location and orientationRouting load, abrasion or pressure-related deformation
ID, OD and wall measurementsIncorrect size, local wear or ovalization
Temperature and pressure historyContinuous load versus short abnormal event
Fluid and cleaning informationCompatibility issue versus external contamination
Lot label and retained sampleInstallation-specific issue versus batch comparison

Agree the scope of any returned-sample inspection, retained evidence and required records before review. A returned sample can be compared with a retained drawing or approved sample, but a root-cause conclusion requires information from the operating system as well as the tube.

Frequently Asked Questions

Does a surface mark always make PTFE tubing unusable?

Not always. Location, depth, wall remaining and service conditions matter. Critical applications require inspection against an agreed acceptance standard.

Why does a replacement tube fail in the same place?

The route, clamp, fitting load, heat or vibration may be unchanged. Correct the system cause before replacement.

Can Pengrowth review a failed sample?

Yes. Send the drawing, batch information, operating conditions, photos and retained samples for an initial review.

Need Help With a PTFE Tubing Problem?

Send clear photos, dimensions and operating conditions so the tube and installation can be reviewed together.

Submit a Troubleshooting Inquiry