PTFE tubing is often considered for chemically demanding vacuum lines, but chemical compatibility alone does not confirm mechanical suitability. External pressure can ovalize or collapse a thin wall, especially at elevated temperature, long unsupported spans or tight bends.
Why Vacuum Loads a Tube Differently
Internal pressure pushes the wall outward. Vacuum creates an external pressure difference that pushes inward. A tube may therefore have acceptable chemical resistance but insufficient resistance to ovalization. Larger OD and thinner wall generally require more care.
| Factor | Vacuum concern | Information to send |
|---|---|---|
| ID, OD and wall | Controls resistance to ovalization | Nominal values and tolerances |
| Temperature | Heat can increase flexibility and creep | Continuous and peak temperature |
| Unsupported length | Long spans can sag or vibrate | Clamp and support drawing |
| Bend radius | A tight bend already reduces bore shape | Minimum available radius |
| Vacuum cycle | Repeated loading may move fittings | Level, duration and cycles |
Wall Thickness and Bore Retention
Specify the minimum acceptable wall and the permitted bore reduction. Do not select only by OD if flow passage is critical. A prototype can be checked on the actual routing fixture before production release. Custom ID and OD can be reviewed on the PTFE extruded tubing page.
Temperature, Bends and Supports
Elevated temperature can reduce stiffness, while a tight bend creates an oval section before vacuum is applied. Provide gradual routing and sufficient support without crushing the tube. The bend radius guide explains routing risks.
Connections and Leak Paths
Leaks can occur at ferrules, flares, barbs, threaded adapters or damaged tube ends. A vacuum leak may draw air inward without showing liquid outside. Use a clean square cut, correct insertion depth and a fitting designed for the selected dimensions. See the connection and fittings guide.
When Another Hose Construction May Be Better
If the line needs repeated movement, external reinforcement or a very tight route, review whether corrugated or braided construction is more appropriate. The assembly must still be checked for vacuum, temperature, cleanliness and fitting compatibility.
- Absolute pressure or vacuum level and units
- Continuous or intermittent operation
- ID, OD, minimum wall and length
- Temperature and chemical medium
- Bends, supports and unsupported span
- Fittings and leak-test method
- Required cleanliness and packaging
Vacuum Application Review Checklist
Pengrowth does not assign a vacuum capability from resin type alone. A useful review combines the actual tube size, wall, unsupported span, bend radius, temperature, connection style and required vacuum level. Large bores, thin walls and hot service generally require more careful bore-retention testing.
| Observation | Possible cause | Review action |
|---|---|---|
| Bore narrows on straight run | Wall or support is insufficient | Review wall, span and external support |
| Flattening occurs only at bends | Ovalization under external pressure | Increase radius or change routing |
| Vacuum decays with shape unchanged | Connection or surface leak path | Isolate fittings and test the tube separately |
| Failure appears only when hot | Reduced stiffness and creep | Repeat the test at service temperature |
For a quotation, include a routing sketch and identify any point where the tube enters a fitting, clamp or heated zone. A short prototype assembly is more informative than a loose material sample when collapse resistance is critical.
Frequently Asked Questions
Can any PTFE tube be used under vacuum?
No. Suitability depends on size, wall, temperature, routing, supports and vacuum level.
Why does the bore flatten at a bend?
The bend creates ovalization, and external pressure can increase it. Use a wider radius or review another geometry.
How should a vacuum line be tested?
Test the complete routed assembly with the real fittings, temperature and cycle duration using an appropriate leak and bore-retention method.
Request a Vacuum Tubing Review
Send the vacuum level, tube dimensions and routing drawing. Pengrowth will review custom manufacturing requirements.